Mechanical Testing - Impact Test 11:51 PM / 0 Before looking at impact testing let us first define what is meant by 'toughness' since the impact test is only one method by whic... Read more »
Mechanical testing - Tensile Test 3:00 PM / 6 Mechanical testing is carried out to produce data that may be used for design purposes or as part of a material joining procedure or oper... Read more »
Wormholes / Crater Pipe 11:42 PM / 0 Elongated pores or wormholes Characteristically, wormholes are elongated pores (Fig. 3) which produce a herring bone appearance on the r... Read more »
Porosity - Weld Defects 11:07 PM / 0 The characteristic features and principal causes of porosity imperfections are described. Best practice guidelines are given so welders ca... Read more »
API ICP Computer-based testing launches in 2014 12:50 PM / 0 Starting in March 2014, the American Petroleum Institute Inspector Certification Program (API ICP) changed its examination delivery method... Read more »
Geometric Shape Imperfections 7:46 PM / 1 This article looks at those imperfections related to poor geometric shape and will concentrate on the following: Excess weld metal ... Read more »
Root Concavity - Suck Back 7:44 PM / 0 A shallow groove that may occur in the root of a butt weld. Common causes Root concavity is caused by shrinkage of the weld pool in t... Read more »